冷旋锻变形对TB9钛合金显微组织和拉伸性能的影响
任德春1,2,苏虎虎1,2,张慧博1,王健1,金伟1,2(),杨锐1,2
Effect of Cold Rotary-Swaging Deformation on Microstructure and Tensile Properties of TB9 Titanium Alloy
Dechun REN1,2,Huhu SU1,2,Huibo ZHANG1,Jian WANG1,Wei JIN1,2(),Rui YANG1,2

图5. 冷旋锻变形后TB9钛合金显微组织的TEM像和70%冷旋锻变形量时的SAED花样

Fig.5. TEM images of TB9 titanium alloy under cold rotary-swaging rates of 15% (a), 35% (b), 70% (c), and SAED pattern of bright band under 70% cold rotary-swaging rate (d) (Inset in Fig.5c show the SAED pattern of dark band)