冷旋锻变形对TB9钛合金显微组织和拉伸性能的影响
任德春1,2,苏虎虎1,2,张慧博1,王健1,金伟1,2(),杨锐1,2
Effect of Cold Rotary-Swaging Deformation on Microstructure and Tensile Properties of TB9 Titanium Alloy
Dechun REN1,2,Huhu SU1,2,Huibo ZHANG1,Jian WANG1,Wei JIN1,2(),Rui YANG1,2

图3. TB9钛合金冷旋锻变形后显微组织OM像和EBSD分析

Fig.3. OM images (a~c) and EBSD analyses (d~f) of TB9 titanium alloy under cold rotary-swaging rates of 15% (a, d), 35% (b, e) and 70% (c, f) (RS—rotary-swaging direction)