[an error occurred while processing this directive]
SO42-对模拟孔隙液中Q235B钢筋腐蚀行为的影响
李恺强1,杨璐嘉2,徐云泽1(),王晓娜3,黄一1
Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution
Kaiqiang LI1,Lujia YANG2,Yunze XU1(),Xiaona WANG3,Yi HUANG1

图1. 不同pH值和不同SO42-浓度的模拟孔隙液中Q235钢的阳极极化曲线

Fig.1. The anodic polarization curves of Q235B steel under different SO42- concentration in the simulated pore solution with pH=12.6 (a), 12.0 (b), 11.0 (c) and 10.0 (d) (i—current density, E—voltage)