SO42-对模拟孔隙液中Q235B钢筋腐蚀行为的影响
李恺强1,杨璐嘉2,徐云泽1(),王晓娜3,黄一1
Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution
Kaiqiang LI1,Lujia YANG2,Yunze XU1(),Xiaona WANG3,Yi HUANG1

图9. D~F组实验完成后电极的表面形貌SEM像

Fig.9. The electrodes SEM image of the surface morphology in the groups D~F after test(a) D-1 (b) D-2 (c) E-1 (d) E-2 (e) F-1 (f) F-2