SO42-对模拟孔隙液中Q235B钢筋腐蚀行为的影响
李恺强1,杨璐嘉2,徐云泽1(),王晓娜3,黄一1
Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution
Kaiqiang LI1,Lujia YANG2,Yunze XU1(),Xiaona WANG3,Yi HUANG1

图7. A~C组实验完成后电极的表面形貌SEM像

Fig.7. The electrode SEM images of the surface morphology in the groups A~C after test(a) A-1 (b) A-2 (c) B-1 (d) B-2 (e) C-1 (f) C-2