SO42-对模拟孔隙液中Q235B钢筋腐蚀行为的影响
李恺强1,杨璐嘉2,徐云泽1(),王晓娜3,黄一1
Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution
Kaiqiang LI1,Lujia YANG2,Yunze XU1(),Xiaona WANG3,Yi HUANG1

图3. 用于阻抗拟合的等效电路图

Fig.3. Equivalent circuit for EIS measurement results fitting shown in Fig.2 (Rs—solution resistance, Rf—film resistance, CPE—constant phase angle element)