23Cr-2.2Ni-6.3Mn-0.26N节Ni型双相不锈钢动态再结晶行为研究
邓亚辉,杨银辉(),曹建春,钱昊
Research on Dynamic Recrystallization Behavior of 23Cr-2.2Ni-6.3Mn-0.26N Low Nickel TypeDuplex Stainless Steel
Yahui DENG,Yinhui YANG(),Jianchun CAO,Hao QIAN

图5. 峰值应力与应变速率和变形温度的关系

Fig.5. Relationship between peak stress and strain rate and deformation temperature (α—material constant)(a) lnσp-lnε˙ (b) σp-lnε˙ (c) ln[sinh(ασp)]-lnε˙ (d) ln[sinh(ασp)]-1/T