23Cr-2.2Ni-6.3Mn-0.26N节Ni型双相不锈钢动态再结晶行为研究
|
|
Research on Dynamic Recrystallization Behavior of 23Cr-2.2Ni-6.3Mn-0.26N Low Nickel TypeDuplex Stainless Steel
|
|
图1. 相同应变速率、不同变形温度条件下的真应力-真应变曲线 |
Fig.1. True stress-true strain curves under the same strain rate and different deformation temperatures(a) 0.01 s-1 (b) 0.1 s-1 (c) 1 s-1 (d) 10 s-1 |
![]() |