23Cr-2.2Ni-6.3Mn-0.26N节Ni型双相不锈钢动态再结晶行为研究
邓亚辉,杨银辉,曹建春,钱昊

Research on Dynamic Recrystallization Behavior of 23Cr-2.2Ni-6.3Mn-0.26N Low Nickel TypeDuplex Stainless Steel
Yahui DENG,Yinhui YANG,Jianchun CAO,Hao QIAN
表1 双相不锈钢的特征参数
Table1 The characteristic parameters of duplex stainless steels
ε˙ / s-1T / Kεcεpσc / MPaσp / MPaσs / MPa
0.110730.145260.26283248.750274.1315269.2720
11730.120750.20557182.550196.3656175.3600
13230.100910.1577784.07686.157175.0038
14230.083830.1237153.27654.715047.8533
110730.160510.33020312.590340.7937333.6438
11730.130120.20899297.210303.6478291.0098
13230.116010.20568123.460128.2068121.7003
14230.106820.1957889.24290.459681.5782
1010730.160030.30253377.082397.2519372.7911
11730.128700.24051334.830346.5571318.7496
13230.080130.11041204.780211.6203198.3243
14230.071020.09170116.350119.3346117.2951