固溶温度对Mn-N型双相不锈钢拉伸变形行为的影响
|
|
Effect of Solution Temperature on Tensile Deformation Behavior of Mn-N Bearing Duplex Stainless Steel
|
|
图1. Mn-N合金化双相不锈钢拉伸样品尺寸 |
Fig.1. Dimension of Mn-N bearing duplex stainless steels (DSSs) specimen for tensile test (unit: mm. RD—rolling direction, TD—transverse direction) |
![]() |