合金元素对顶头钢氧化行为的影响
郑成明,田青超

Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel
Chengming ZHENG,Qingchao TIAN
表1 实验材料的化学成分
Table1 The chemical compositions of experimental materials
MaterialCSiMnCrNiMoVFe
20Cr2Ni30.200.701.502.002.60--Bal.
30Cr3Ni-Mo2V

0.30

0.20

0.40

3.00

0.90

2.00

0.50

Bal.

H130.400.801.005.500.101.551.30Bal.