合金元素对顶头钢氧化行为的影响
|
|
Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel
|
|
图6. H13内、外层氧化膜形貌及线扫描结果 |
Fig.6. Morphology of oxide scale showing transmission "venation" in H13 and its line scan spectra from I to II in the inner oxide scale (a) and bright white substance in the external oxide scale (b) |
![]() |