高合金化GH4065镍基变形高温合金点状偏析研究
王资兴,黄烁,张北江,王磊,赵光普

Study on Freckle of a High-Alloyed GH4065 Nickel Base Wrought Superalloy
Zixing WANG,Shuo HUANG,Beijiang ZHANG,Lei WANG,Guangpu ZHAO
表3 GH4065合金点偏凝固过程与热力学平衡状态的第二相热力学统计
Table 3 Thermodynamic statistics of the secondary phase in the GH4065 alloy during solidification process and at thermodynamic equilibrium
PhasePositionSolidificationThermodynamic
Precipitated beginning Tem. / ℃Mass fraction / %Solidus Tem. / ℃Mass fraction / %
γFreckle1294.8Bal.1294.8Bal.
Matrix1350.5Bal.1350.5Bal.
γ′Freckle1160.039.01134.140.8
Matrix1100.930.01108.638.3
ηFreckle1220.08.81215.217.7
Matrix1196.21.3-0
M2B3Freckle1150.00.261112.80.62
Matrix1178.20.101098.10.18
MCFreckle1282.10.371282.30.41
Matrix1265.00.0741272.70.081