高合金化GH4065镍基变形高温合金点状偏析研究
王资兴
1,
2
,黄烁
3
,张北江
3
,王磊
1
(
),赵光普
3
Study on Freckle of a High-Alloyed GH4065 Nickel Base Wrought Superalloy
Zixing WANG
1,
2
,Shuo HUANG
3
,Beijiang ZHANG
3
,Lei WANG
1
(
),Guangpu ZHAO
3
图7.
GH4065合金点偏晶粒取向差分布统计图
Fig.7.
EBSD misorientation distributions chart of theGH4065 alloy freckle