磁场对含CaO铁氧化物还原的影响
金永丽1,2,于海2,张捷宇1,赵增武3()
Effects of Magnetic Field on Reduction of CaOContaining Iron Oxides
Yongli JIN1,2,Hai YU2,Jieyu ZHANG1,Zengwu ZHAO3()

图2. 纯Fe2O3和Fe2O3+2.5%CaO体系等温还原度曲线图

Fig.2. Isothermal reduction curves of pure Fe2O3 and Fe2O3+2.5%CaO systems in a constant magnetic field (CMF) 1.02 T, and under the normal condition (NC) without a magnetic field applied