[an error occurred while processing this directive]
磁场对含CaO铁氧化物还原的影响
金永丽1,2,于海2,张捷宇1,赵增武3()
Effects of Magnetic Field on Reduction of CaOContaining Iron Oxides
Yongli JIN1,2,Hai YU2,Jieyu ZHANG1,Zengwu ZHAO3()

图1. 磁场还原炉示意图

Fig.1. Schematic of magnetic field reduction furnace (1—gas cylinder, 2—moisture filter, 3—oxygen filter, 4—mass flow controller, 5—gas mixer, 6—Al2O3 work tube with heating elements wrapped around the tube, 7—heat insulation cover, 8—water cooling jacket, 9—permanent magnet, 10—thermocouple, 11—sliding rail for moving heat insulation cover (7) and magnet (9), 12—furnace temperature controller)