弥散固态颗粒对Al-Bi合金液-液相分离过程的影响
张林,满田囡,王恩刚(
)
Influence of Dispersed Solid Particles on the Liquid-Liquid Separation Process of Al-Bi Alloys
Lin ZHANG,Tiannan MAN,Engang WANG(
)
图3.
Al-Bi-Ce合金的SEM像和EDS分析
Fig.3.
SEM image (a) and EDS analyses (b) of Al-Bi-Ce alloy