[an error occurred while processing this directive]
Er对Mg-5Zn-xEr镁合金热裂敏感性的影响
刘耀鸿,王朝辉(),刘轲,李淑波,杜文博
Effects of Er on Hot Cracking Susceptibility of Mg-5Zn-xEr Magnesium Alloys
Yaohong LIU,Zhaohui WANG(),Ke LIU,Shubo LI,Wenbo DU

图8. Mg-5Zn-xEr合金的凝固曲线(临界尺寸法实验)

Fig.8. Solidification curves of Mg-5Zn-xEr alloys (Experiment via critical size method)(a) x=0.83 (b) x=1.25 (c) x=2.5 (d) x=5