焊接线能量对5182-O/HC260YD+Z异种材料CMT搭接接头组织与性能的影响
吉华1,2,邓运来3(),徐红勇2,郭伟强2,邓建峰2,范世通3
The Influence of Welding Line Energy on the Microstructure and Property of CMT Overlap Joint of 5182-Oand HC260YD+Z
Hua JI1,2,Yunlai DENG3(),Hongyong XU2,Weiqiang GUO2,Jianfeng DENG2,Shitong FAN3

图3. 铝合金/钢CMT搭接接头不同区域微区XRD谱(S3)

Fig.3. XRD spectra of different regions of an Al alloy/steel CMT lap joint (S3)