焊接线能量对5182-O/HC260YD+Z异种材料CMT搭接接头组织与性能的影响
|
|
The Influence of Welding Line Energy on the Microstructure and Property of CMT Overlap Joint of 5182-Oand HC260YD+Z
|
|
图8. 图7面扫描分析结果 |
Fig.8. EDS mapping analyses of Fig.7c (a) and Fig.7d (b) |
![]() |