焊接线能量对5182-O/HC260YD+Z异种材料CMT搭接接头组织与性能的影响
吉华1,2,邓运来3(),徐红勇2,郭伟强2,邓建峰2,范世通3
The Influence of Welding Line Energy on the Microstructure and Property of CMT Overlap Joint of 5182-Oand HC260YD+Z
Hua JI1,2,Yunlai DENG3(),Hongyong XU2,Weiqiang GUO2,Jianfeng DENG2,Shitong FAN3

图6. 送丝速率、焊接速率对熔焊界面微观形貌的影响

Fig.6. Microstructures of the fusion interface zones under different wire feed speeds and welding speeds(a) S1 (b) S3 (c) partial magnification of the area in Fig.6b (d) S5 (e) S6 (f) S9