Ni-Mn-Ga-Ti铁磁形状记忆合金的相稳定性和磁性能的第一性原理计算
|
|
First-Principles Calculations of Phase Stability and Magnetic Properties of Ni-Mn-Ga-Ti FerromagneticShape Memory Alloys
|
|
图4. Ni8Mn4-xGa4Tix (x=0、1、2)合金奥氏体母相的自旋分波态密度 |
Fig.4. Partial density of states of ferromagnetic austenite for Ni8Mn4-xGa4Tix alloys with x=0 (a), x=1 (b) and x=2 (c) |
![]() |