基于磁畴结构交互作用的激光刻痕取向硅钢磁致伸缩系数计算
|
Calculation of Magnetostriction Coefficient for Laser-Scribed Grain-Oriented Silicon Steel Based onMagnetic Domain Interaction
|
图2. 不同磁畴能量和刻痕区杂散磁场能与刻痕能量密度(Ea)的关系 |
Fig.2. Domain energies (Emain, Elancet, Eclosure) and stray field energy (EstT) as a function of laser energy density (Ea) (Emain—energy of 180° domain wall, Elancet—energy of lancet domain system, Eclosure—energy of closure domain system, β—orientation deviation angle, Dp—laser-scribing spacing, D2—laser-scribed width) |
![]() |