G20Mn5N铸钢件微细观孔洞三维特征及形态演化
|
Three-Dimensional Characteristics and Morphological Evolution of Micro/Meso Pores inG20Mn5N Steel Castings
|
图8. 轴向拉伸载荷作用下试样4标距段孔洞的X射线三维成像结果 |
Fig.8. Pores inspected with 3D X-ray tomography technology in the gauge section of specimen 4 during the uniaxial tensile loading(a) εAxial=0.214 (b) εAxial=0.343 (c) εAxial=0.422 (d) εAxial=0.460 |
![]() |