淬火配分贝氏体钢不同位置残余奥氏体C、Mn元素表征及其稳定性
|
|
C and Mn Elements Characterization and Stability of Retained Austenite in Different Locations ofQuenching and Partitioning Bainite Steels
|
|
图6. IQ&PB工艺处理后试样的XRD谱 |
Fig.6. XRD spectrum of sample after the treatment of IQ&PB process |
![]() |