淬火配分贝氏体钢不同位置残余奥氏体C、Mn元素表征及其稳定性
|
|
C and Mn Elements Characterization and Stability of Retained Austenite in Different Locations ofQuenching and Partitioning Bainite Steels
|
|
图5. IQ&PB工艺处理后试样中C、Mn元素分布 |
Fig.5. Microstructure (a) and EPMA images of C (b) and Mn (c) elements of sample after the treatment of IQ&PB process (A—area fraction, Aver.—average) |
![]() |