淬火配分贝氏体钢不同位置残余奥氏体C、Mn元素表征及其稳定性
|
|
C and Mn Elements Characterization and Stability of Retained Austenite in Different Locations ofQuenching and Partitioning Bainite Steels
|
|
图3. IQ&PB工艺处理后试样的SEM像 |
Fig.3. SEM images of sample after the treatment of IQ&PB process (F—ferrite, B—bainite, M/A—martensite/austenite) |
![]() |