0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3铁电薄膜90°分步畴转与温度效应
|
|
PFM Study of the 90° Step-by-Step Domain Switching and the Temperature Effect in 0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3 Ferroelectric Thin Film
|
|
图5. 电畴翻转速率随直流偏压的变化 |
Fig.5. The c- domain area portion dependence on scanning time at the tip bias voltages of 5 and 8 V |
![]() |