0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3铁电薄膜90°分步畴转与温度效应
|
|
PFM Study of the 90° Step-by-Step Domain Switching and the Temperature Effect in 0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3 Ferroelectric Thin Film
|
|
图7. 压电响应信号随温度的变化 |
Fig.7. Variation of piezoresponse (PR) contrast of the 0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3 thin film with temperature |
![]() |