0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3铁电薄膜90°分步畴转与温度效应
|
|
PFM Study of the 90° Step-by-Step Domain Switching and the Temperature Effect in 0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3 Ferroelectric Thin Film
|
|
图6. 不同温度0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3薄膜铁电纳米畴结构PFM像 |
Fig.6. PFM images of the 0.8PbTiO3-0.2Bi(Mg0.5Ti0.5)O3 thin film at 28 ℃ (a), 50 ℃ (b), 70 ℃ (c) and 90 ℃ (d) |
![]() |