含Cu界面层碳纤维增强铝基复合材料制备工艺及其力学性能研究
|
|
Fabrication and Mechanical Properties of Carbon Fiber-Reinforced Aluminum Matrix Compositeswith Cu Interphase
|
|
图8. 纯Al和Cf/Al复合材料拉伸工程应力-应变曲线 |
Fig.8. Tensile engineering stress-strain curves for pure Al and Cf/Al composites |
![]() |