含Cu界面层碳纤维增强铝基复合材料制备工艺及其力学性能研究
|
|
Fabrication and Mechanical Properties of Carbon Fiber-Reinforced Aluminum Matrix Compositeswith Cu Interphase
|
|
图1. 碳纤维表面电镀Cu界面层实验装置示意图 |
Fig.1. Schematic of experiment setup used for the electroplating of Cu interphase on carbon fibers |
![]() |