含Cu界面层碳纤维增强铝基复合材料制备工艺及其力学性能研究
|
|
Fabrication and Mechanical Properties of Carbon Fiber-Reinforced Aluminum Matrix Compositeswith Cu Interphase
|
|
图5. Cf/Al复合材料的微观形貌 |
Fig.5. SEM image of Cf/Al composites (a) and the magnified image of selected area in Fig.5a (b) |
![]() |