含Cu界面层碳纤维增强铝基复合材料制备工艺及其力学性能研究
|
|
Fabrication and Mechanical Properties of Carbon Fiber-Reinforced Aluminum Matrix Compositeswith Cu Interphase
|
|
图2. 采用真空压力浸渗法制备碳纤维增强铝基(Cf/Al)复合材料的工艺示意图 |
Fig.2. Schematic for the fabrication of carbon fiber-reinforced aluminum matrix (Cf/Al) composites |
![]() |