双脉冲HiPIMS放电特性及CrN薄膜高速率沉积
|
|
Discharge Characteristics of Novel Dual-Pulse HiPIMS and Deposition of CrN Films with High Deposition Rate
|
|
图5. 双脉冲HiPIMS引燃脉冲电压及HiPIMS条件对单位功率基体电流积分的影响 |
Fig.5. Influence of ignition pulse voltage of dual-pulse HiPIMS and conventional HiPIMS on the substrate current integral at unit power |
![]() |