双脉冲HiPIMS放电特性及CrN薄膜高速率沉积
吴厚朴,田修波(),张新宇,巩春志
Discharge Characteristics of Novel Dual-Pulse HiPIMS and Deposition of CrN Films with High Deposition Rate
Houpu WU,Xiubo TIAN(),Xinyu ZHANG,Chunzhi GONG

图4. 双脉冲HiPIMS不同引燃脉冲电压及HiPIMS条件下基体电流波形图

Fig.4. Waveforms of substrate current for conventional HiPIMS and dual-pulse HiPIMS with different ignition voltages