双脉冲HiPIMS放电特性及CrN薄膜高速率沉积
|
|
Discharge Characteristics of Novel Dual-Pulse HiPIMS and Deposition of CrN Films with High Deposition Rate
|
|
图10. 双脉冲HiPIMS引燃脉冲电压对CrN薄膜晶粒尺寸的影响 |
Fig.10. Influence of ignition pulse voltage of dual-pulse HiPIMS on the grain size of CrN coatings |
![]() |