静水压力对超纯Al/超纯Fe电偶中超纯Al腐蚀行为的影响 |
||||||||||||||||||||||||
| 马荣耀,穆鑫,刘博,王长罡,魏欣,赵林,董俊华,柯伟 | ||||||||||||||||||||||||
|
Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe |
||||||||||||||||||||||||
| Rongyao MA,Xin MU,Bo LIU,Changgang WANG,Xin WEI,Lin ZHAO,Junhua DONG,Wei KE | ||||||||||||||||||||||||
| 表1 不同静水压力下,由Weibull分布图的线性部分确定的超纯Al/超纯Fe电偶对在3.5%NaCl中的形状参数(m)和尺度参数(n) | ||||||||||||||||||||||||
| Table 1 The shape parameter (m) and the scale parameter (n) determined from the linear slope of ln{ln[l/(l-F(1/fn))]} vs ln(1/fn) plot for coupled pairs of ultrapure Al and ultrapure Fe in 3.5%NaCl at different hydrostatic pressures | ||||||||||||||||||||||||
|
||||||||||||||||||||||||