[an error occurred while processing this directive]
静水压力对超纯Al/超纯Fe电偶中超纯Al腐蚀行为的影响
马荣耀1,2,穆鑫1,刘博3,王长罡1,魏欣1,赵林1,董俊华1(),柯伟1
Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe
MA Rongyao1,2,MU Xin1,LIU Bo3,WANG Changgang1,WEI Xin1,ZHAO Lin1,DONG Junhua1(),KE Wei1

图8. 不同静水压力下,超纯Al/超纯Fe电偶对在3.5%NaCl中的腐蚀事件发生频率(fn)和腐蚀事件平均电量(q)随时间的变化

Fig.8. Plot of the frequency of events (fn) versus time (a) and plot of the average charge in each event (q) versus time (b) for coupled pairs of ultrapure Al and ultrapure Fe in 3.5%NaCl at different hydrostatic pressures