静水压力对超纯Al/超纯Fe电偶中超纯Al腐蚀行为的影响
马荣耀1,2,穆鑫1,刘博3,王长罡1,魏欣1,赵林1,董俊华1(),柯伟1
Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe
MA Rongyao1,2,MU Xin1,LIU Bo3,WANG Changgang1,WEI Xin1,ZHAO Lin1,DONG Junhua1(),KE Wei1

图7. 不同静水压力下,超纯Al/超纯Fe电偶对在3.5%NaCl中的噪声电阻(Rn)随时间的变化曲线和累积概率曲线

Fig.7. Plot of noise resistance (Rn) versus time (a) and cumulative probability plot of Rn(b) for coupled pairs of ultrapure Al and ultrapure Fe in 3.5%NaCl at different hydrostatic pressures