静水压力对超纯Al/超纯Fe电偶中超纯Al腐蚀行为的影响
马荣耀1,2,穆鑫1,刘博3,王长罡1,魏欣1,赵林1,董俊华1(),柯伟1
Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe
MA Rongyao1,2,MU Xin1,LIU Bo3,WANG Changgang1,WEI Xin1,ZHAO Lin1,DONG Junhua1(),KE Wei1

图5. 不同静水压力下,经DWT去直流漂移前后超纯Al/超纯Fe电偶对在3.5%NaCl中的电偶电流噪声(ECN)谱

Fig.5. Galvanic current noise (ECN) spectra of coupled pairs of ultrapure Al and ultrapure Fe in 3.5%NaCl before (a) and after (b) a DC drift remove by using DWT at different hydrostatic pressures