[an error occurred while processing this directive]
静水压力对超纯Al/超纯Fe电偶中超纯Al腐蚀行为的影响
马荣耀1,2,穆鑫1,刘博3,王长罡1,魏欣1,赵林1,董俊华1(),柯伟1
Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe
MA Rongyao1,2,MU Xin1,LIU Bo3,WANG Changgang1,WEI Xin1,ZHAO Lin1,DONG Junhua1(),KE Wei1

图3. 0.1和10 MPa下在3.5%NaCl中超纯Al和超纯Fe的极化曲线

Fig.3. Electrodynamic polarization curves of ultrapure Al and ultrapure Fe in 3.5%NaCl at hydrostatic pressures of 0.1 and 10 MPa (iFe,a and iFe,c—anode and cathode current densities of Fe dissolution reaction at -740 mV respectively, i'Fe,a and i'Fe,c—anode and cathode current densities of Fe dissolution reaction at -750 mV respectively)