Q&P钢热处理过程有限元法数值模拟模型研究
张清东,林潇,刘吉阳(),胡树山
Modelling of Q&P Steel Heat Treatment Process Based on Finite Element Method
ZHANG Qingdong,LIN Xiao,LIU Jiyang(),HU Shushan

图16. Q&P热处理过程各阶段试样变形模拟值与实测值对比

Fig.16. Comparisons between simulated and measured deformations of samples in different stages of Q&P heat treatment process(a) first quenching process (b) partitioned heating process(c) partitioned holding process (d) second quenching process