Q&P钢热处理过程有限元法数值模拟模型研究
张清东,林潇,刘吉阳(),胡树山
Modelling of Q&P Steel Heat Treatment Process Based on Finite Element Method
ZHANG Qingdong,LIN Xiao,LIU Jiyang(),HU Shushan

图9. 不同淬火温度Q&P热处理第二次淬火过程的相变动力学曲线

Fig.9. Phase change kinetics curves of the second quenching process with different quenching temperature Q&P heat treatment