Q&P钢热处理过程有限元法数值模拟模型研究
张清东,林潇,刘吉阳(),胡树山
Modelling of Q&P Steel Heat Treatment Process Based on Finite Element Method
ZHANG Qingdong,LIN Xiao,LIU Jiyang(),HU Shushan

图8. 不同淬火温度下第二次淬火过程前后的组织变化

Fig.8. Microstructure changes before and after the second quenching process with different quenching temperatures