Q&P
钢热处理过程有限元法数值模拟模型研究
张清东,林潇,刘吉阳(
),胡树山
Modelling of Q&P Steel Heat Treatment Process Based on Finite Element Method
ZHANG Qingdong,LIN Xiao,LIU Jiyang(
),HU Shushan
图4.
相变塑性实验方案
Fig.4.