Q&P钢热处理过程有限元法数值模拟模型研究
张清东,林潇,刘吉阳(),胡树山
Modelling of Q&P Steel Heat Treatment Process Based on Finite Element Method
ZHANG Qingdong,LIN Xiao,LIU Jiyang(),HU Shushan

图1. 淬火-分配(Q&P) QP980高强钢的连续冷却实验方案及CCT曲线

Fig.1. Experimental scheme (a) and continuous cooling transformation (CCT) curves (b) of continuous cooling of quenching and partitioning (Q&P) QP980 steel (A—austenite, B—bainite, F—ferrite, M—martensite)