纳米晶化对锆基非晶合金动态压缩性能的影响 |
|||||||||||||||
| 金辰日,杨素媛,邓学元,王扬卫,程兴旺 | |||||||||||||||
|
Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy |
|||||||||||||||
| Chenri JIN,Suyuan YANG,Xueyuan DENG,Yangwei WANG,Xingwang CHENG | |||||||||||||||
| 表1 退火态锆基非晶合金的晶化放热焓和晶化相体积分数 | |||||||||||||||
| Table 1 Crystallization exothermic enthalpy (ΔH) and volume fraction of crystallized phase (χ) of annealed Zr-based amorphous alloy | |||||||||||||||
|
|||||||||||||||