[an error occurred while processing this directive]
纳米晶化对锆基非晶合金动态压缩性能的影响
金辰日1,杨素媛1,2(),邓学元1,王扬卫1,2,程兴旺1,2
Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy
JIN Chenri1,YANG Suyuan1,2(),DENG Xueyuan1,WANG Yangwei1,2,CHENG Xingwang1,2

图8. 退火态锆基非晶合金压缩断口形貌

Fig.8. Compression fracture morphologies of annealed Zr-based amorphous alloy with holding time of 20 min (a1~a6), 40 min (b1~b4), 60 min (c1~c5) and 80 min (d1~d6) under different strain rates of 1×10-3 s-1 (a1, a2, b1, b2, c1, c2, d1, d2, d3), 1×103 s-1 (a3, a4, b3, c3, d4) and 3×103 s-1 (a5, a6, b4, c4, c5, d5, d6)