激光多次熔凝Zr55Cu30Al10Ni5非晶合金的晶化形态与演化机理
杨高林1,林鑫2(),卢献钢1
Crystallization Morphology and Evolution Mechanism of Laser Multiple Remelting of Zr55Cu30Al10Ni5 Metallic Glass
YANG Gaolin1,LIN Xin2(),LU Xiangang1

图8. 激光多次熔凝No.B和No.C非晶合金板过程中的晶粒直径演化

Fig.8. Variation of spherulitic crystallization diameters during multiple laser remelting No.B and No.C metallic glass plates